Decay threshold of acetylated rattan (Calamus manan) against soft rot

Allbwn ymchwil: Cyfraniad at gyfnodolynErthygladolygiad gan gymheiriaid

StandardStandard

Decay threshold of acetylated rattan (Calamus manan) against soft rot. / Hamid, N.H.; Hale, M.D.
Yn: Journal of Forestry Research, Cyfrol 24, Rhif 2, 28.04.2013, t. 375-380.

Allbwn ymchwil: Cyfraniad at gyfnodolynErthygladolygiad gan gymheiriaid

HarvardHarvard

Hamid, NH & Hale, MD 2013, 'Decay threshold of acetylated rattan (Calamus manan) against soft rot', Journal of Forestry Research, cyfrol. 24, rhif 2, tt. 375-380. https://doi.org/10.1007/s11676-013-0362-9

APA

Hamid, N. H., & Hale, M. D. (2013). Decay threshold of acetylated rattan (Calamus manan) against soft rot. Journal of Forestry Research, 24(2), 375-380. https://doi.org/10.1007/s11676-013-0362-9

CBE

MLA

Hamid, N.H. a M.D. Hale. "Decay threshold of acetylated rattan (Calamus manan) against soft rot". Journal of Forestry Research. 2013, 24(2). 375-380. https://doi.org/10.1007/s11676-013-0362-9

VancouverVancouver

Hamid NH, Hale MD. Decay threshold of acetylated rattan (Calamus manan) against soft rot. Journal of Forestry Research. 2013 Ebr 28;24(2):375-380. doi: 10.1007/s11676-013-0362-9

Author

Hamid, N.H. ; Hale, M.D. / Decay threshold of acetylated rattan (Calamus manan) against soft rot. Yn: Journal of Forestry Research. 2013 ; Cyfrol 24, Rhif 2. tt. 375-380.

RIS

TY - JOUR

T1 - Decay threshold of acetylated rattan (Calamus manan) against soft rot

AU - Hamid, N.H.

AU - Hale, M.D.

PY - 2013/4/28

Y1 - 2013/4/28

N2 - We investigated the resistance of acetylated rattan against soft rot and other soil inhabiting micro-organisms in comparison with wood of beech and Scots pine. Calamus manan of 10 and 13 years old under rubber tree canopy was acetylated to different levels by reaction times (0.25 to 30 hours) and was tested for soft rot decay for 32 weeks. Acetylated rattan at decay protection thresholds of 15.4% and 16.2% weight gain (WG) were fully protected, as shown by both weight loss and strength loss criteria. The static bending properties of untreated rattan decayed by soft rot were significantly lower than for acetylated rattan.

AB - We investigated the resistance of acetylated rattan against soft rot and other soil inhabiting micro-organisms in comparison with wood of beech and Scots pine. Calamus manan of 10 and 13 years old under rubber tree canopy was acetylated to different levels by reaction times (0.25 to 30 hours) and was tested for soft rot decay for 32 weeks. Acetylated rattan at decay protection thresholds of 15.4% and 16.2% weight gain (WG) were fully protected, as shown by both weight loss and strength loss criteria. The static bending properties of untreated rattan decayed by soft rot were significantly lower than for acetylated rattan.

U2 - 10.1007/s11676-013-0362-9

DO - 10.1007/s11676-013-0362-9

M3 - Article

VL - 24

SP - 375

EP - 380

JO - Journal of Forestry Research

JF - Journal of Forestry Research

SN - 1007-662x

IS - 2

ER -